Bu, Y.; Li, K.; Ma, Y.; Liang, Z.; Jianliang, Z.; Raabe, D.: Atomistic view of green steel: simulation of early-stage direct reduction of wüstite (FeO) by hydrogen. Chemical Engineering Science 326, 123611 (2026)
Trinca, A.; Verdone, N.; Özgün, Ö.; Ma, Y.; Filho, I.; Raabe, D.; Vilardi, G.: Sustainable ironmaking from low-grade iron ores: A kinetic study on thermal decomposition and reduction of iron (II) oxalate. Journal of Environmental Chemical Engineering 13 (6), 119573 (2025)
Dong, X.; Wei, S.; Tehranchi, A.; Saksena, A.; Ponge, D.; Sun, B.; Raabe, D.: The dual role of boron on hydrogen embrittlement: example of interface-related hydrogen effects in an austenite-ferrite two-phase lightweight steel. Acta Materialia 299, 121458 (2025)
Max Planck team explains dendrite propagation, paving the way for safer and longer-lasting next-generation batteries. They publish their findings in the journal Nature.
International researcher team presents a novel microstructure design strategy for lean medium-manganese steels with optimized properties in the journal Science
Hydrogen embrittlement remains a strong obstacle to the durability of high-strength structural materials, compromising their performance and longevity in critical engineering applications. Of particular relevance is the effect of mobile and trapped hydrogen at interfaces, such as grain and phase boundaries, since they often determine the material’s…