Suchergebnisse
Alle Typen
Zeitschriftenartikel (4354)
3941.
Zeitschriftenartikel
75, S. 20 - 25 (2004)
Hot-Rolling Experiments on Deformation Behaviour of Oxide Scale. Steel Research International 3942.
Zeitschriftenartikel
101, 2-4, S. 139 - 148 (2004)
APFIM Investigations on Site Occupancies of the Ternary Alloying Elements Cr, Fe, and Re in NiAl. Ultramicroscopy 3943.
Zeitschriftenartikel
38, S. 25 - 36 (2004)
Supersaturation of Iron with Nitrogen, Hydrogen or Carbon and the Consequences. Materiali in Tehnologije 3944.
Zeitschriftenartikel
7 (1), S. 89 - 95 (2004)
Role of Alloying Elements and Carbides in the Chlorine-induced Corrosion of Steels and Alloys. Materials Research 3945.
Zeitschriftenartikel
75 (1), S. 38 - 46 (2004)
Initial Oxidation of a 9 % CrMo- and a 12 % CrMoV – Steel. Steel Research International 3946.
Zeitschriftenartikel
446 (1), S. 61 - 71 (2004)
Tailoring of the morphology and chemical composition of thin organosilane microwave plasma polymer layers on metal substrates. Thin Solid Films 3947.
Zeitschriftenartikel
13, 4, S. 240 - 247 (2004)
Surface treatment of NiTi for medical applications. Minimally Invasive Therapy & Allied Technologies 3948.
Zeitschriftenartikel
75, 5, S. 339 - 342 (2004)
Deformation behaviour of iron-rich iron-aluminium alloys with ternary transition metal additions. Steel Research International 3949.
Zeitschriftenartikel
75, 5, S. 343 - 352 (2004)
Microstructure and deformation behaviour of iron-rich iron-aluminium alloys with ternary carbon and silicon additions. Steel Research International 3950.
Zeitschriftenartikel
214 (3), S. 252 - 260 (2004)
Thermal stability of Ti and Pt nanowires manufactured by Ga+ focused ion beam. Journal of Microscopy 3951.
Zeitschriftenartikel
Texture Analysis of a Coarse Grained Fe3Al Cast Alloy by Neutron Scattering. Genf-Experimental Report 2003, S. 183 - 199 (2004)
3952.
Zeitschriftenartikel
467-470, S. 75 - 80 (2004)
Investigation of nucleation mechanisms of recrystallization in warm rolled Fe3Al base alloys. Materials Science Forum 3953.
Zeitschriftenartikel
46, 8 (2004)
Models describing the degradation of FeAl and NiAl alloys induced by ZnCl2/KCl melt at 400-450 °C. Corrosion Science 3954.
Zeitschriftenartikel
461-464, S. 1047 - 1054 (2004)
High temperature interactions of pure Cr with KCl. Materials Science Forum 3955.
Zeitschriftenartikel
75 (11), S. 766 - 772 (2004)
Iron-Rich Iron-Titanium-Silicon Alloys with Strengthening Intermetallic Laves Phase Precipitates. steel research international 3956.
Zeitschriftenartikel
52, S. 3603 - 3612 (2004)
A constitutive model for fcc single crystals based on dislocation densities and its application to uniaxial compression of aluminium single crystals. Acta Materialia 3957.
Zeitschriftenartikel
29, 3, S. 259 - 395 (2004)
Numerical study of textures and Lankford values for FCC polycrystals by use of a modified Taylor model. Computational Materials Science 3958.
Zeitschriftenartikel
12 (12), S. 1345 - 1359 (2004)
Deformation Behaviour and Oxidation Resistance of Single-Phase and Two-Phase L21 Fe–Al–Ti Alloys. Intermetallics 3959.
Zeitschriftenartikel
20, 2 (2004)
Surface modification of various Fe-Si and Fe-Mn alloys by oxidation/reduction treatments. Surface Engineering 3960.
Zeitschriftenartikel
135, S. 52 - 61 (2004)
Development of spinel forming alloys with improved electronic conductivity for MCFC application. Journal of Power Sources