Suchergebnisse
Alle Typen
Zeitschriftenartikel (4325)
3901.
Zeitschriftenartikel
151, 12, S. B621 - B626 (2004)
Scaning Kelvin Probe Force Microscopy: A Useful Tool for Studying Atmospheric Corrosion of MgAl Alloys In Situ. Journal of the Electrochemical Society 3902.
Zeitschriftenartikel
16 (S429) (2004)
Molecular Dynamics Simulations. Journal of Physics: Condensed Matter 3903.
Zeitschriftenartikel
151 (12), S. B621 - B626 (2004)
Scanning Kelvin probe force microscopy - A useful tool for studying atmospheric corrosion of MgAl alloys in situ. Journal of the Electrochemical Society 3904.
Zeitschriftenartikel
6, 8, S. 800 - 804 (2004)
Electrochemical characterizations of precipitates formed on zinc in alkaline sulphate solution with increasing pH values. Electrochemistry Communicatios 3905.
Zeitschriftenartikel
755, 1, S. 5 - 12 (2004)
Thin Strip Casting of Steel with a Twin Roll Caster - Correlation between Feeding System and Strip Quality. Steel Research Int. 3906.
Zeitschriftenartikel
461–464, S. 1055 - 1055 (2004)
Fundamental studies on alkali chloride induced corrosion during combustion of biomass. Materials Science Forum 3907.
Zeitschriftenartikel
36, S. 533 - 539 (2004)
APFIM investigations on the intermetallic Ni49.5Al49.5Re1 alloy. Surface and Interface Analysis 3908.
Zeitschriftenartikel
36, S. 533 - 539 (2004)
Atom probe field ion microscopy investigations on the intermetallic Ni49.5Al49.5Re1 alloy. Surface and Interface Analysis 3909.
Zeitschriftenartikel
95 (6), S. 464 - 468 (2004)
Experimental study and Cluster Variation modelling of the A2/B2 equilibria at the Ti-rich side of the Ti–Fe system. Zeitschrift für Metallkunde 3910.
Zeitschriftenartikel
75 (1), S. 62 - 73 (2004)
Iron-rich iron-aluminium-molybdenum alloys with strengthening intermetallic mu phase and R phase precipitates. Steel Research International 3911.
Zeitschriftenartikel
12 (6), S. 625 - 633 (2004)
Alloys based on Fe3Al or FeAl with strengthening Mo3Al precipitates. Intermetallics 3912.
Zeitschriftenartikel
75, S. 20 - 25 (2004)
Hot-Rolling Experiments on Deformation Behaviour of Oxide Scale. Steel Research International 3913.
Zeitschriftenartikel
101, 2-4, S. 139 - 148 (2004)
APFIM Investigations on Site Occupancies of the Ternary Alloying Elements Cr, Fe, and Re in NiAl. Ultramicroscopy 3914.
Zeitschriftenartikel
38, S. 25 - 36 (2004)
Supersaturation of Iron with Nitrogen, Hydrogen or Carbon and the Consequences. Materiali in Tehnologije 3915.
Zeitschriftenartikel
7 (1), S. 89 - 95 (2004)
Role of Alloying Elements and Carbides in the Chlorine-induced Corrosion of Steels and Alloys. Materials Research 3916.
Zeitschriftenartikel
75 (1), S. 38 - 46 (2004)
Initial Oxidation of a 9 % CrMo- and a 12 % CrMoV – Steel. Steel Research International 3917.
Zeitschriftenartikel
446 (1), S. 61 - 71 (2004)
Tailoring of the morphology and chemical composition of thin organosilane microwave plasma polymer layers on metal substrates. Thin Solid Films 3918.
Zeitschriftenartikel
13, 4, S. 240 - 247 (2004)
Surface treatment of NiTi for medical applications. Minimally Invasive Therapy & Allied Technologies 3919.
Zeitschriftenartikel
75, 5, S. 339 - 342 (2004)
Deformation behaviour of iron-rich iron-aluminium alloys with ternary transition metal additions. Steel Research International 3920.
Zeitschriftenartikel
75, 5, S. 343 - 352 (2004)
Microstructure and deformation behaviour of iron-rich iron-aluminium alloys with ternary carbon and silicon additions. Steel Research International